Sharp, W H (Aluminum Company of America) Moore, R L (Aluminum Company of America)
naca-tn-897
June 1943


Bearing tests of AM-3S, AM-52S, and AM-C57S magnesium-alloy sheet in various thicknesses and tempers were made. Bearing yield and ultimate strengths were determined and compared for various edge distances and for various ratios of loading-pin diameter to sheet thickness. Tensile strengths were determined and ratios of average bearing yield and ultimate strength to tensile strength are given. The results of the tests indicated that ultimate bearing strengths increased with edge distances up to 1.5 to 2 times the diameter of the loading pin; that ultimate bearing strengths are a function of the ratio of pin diameter to sheet thickness; and that these properties are effected only slightly by increases in edge distance greater than 1.5 diameters.